a few words on primers and sealers before I go on...in Cali (where I was born and raised) body shops must use a waterbourne or water based primer (EPA stuff)...not sure if other states have adopted this or not, NC has not (thank god)...in Cali this is fine becuase of the drier climates...
in eastern NC the humidity is unreal (summertime is normally mid 90's F to low 100's F, with humidty around 90% or higher even on clear days, this also brings the heat index (what it actually feels like) up to 115 F. I had sprayed the entire car in a PPG waterbourne primer/sealer...after 2 days in the humidity alone, it began rusting through!! (will try to find pics of this)